Title: One Discussion from the March/April 2010 ACI Structural Journal and Two Discussions from the May/June 2010 ACI Structural Journal

Author(s): Donald F. Meinheit, Neil S. Anderson, and Andor Windisch

Publication: Structural Journal

Volume: 108

Issue: 2

Appears on pages(s): 248-253

Keywords:

DOI: 10.14359/51664262

Date: 3/1/2011

Abstract:
Disc. 107-S14/From the March-April 2010 ACI Structural Journal, p. 146. Shear Behavior of Headed Anchors with Large Diameters and Deep Embedments. Paper by Nam Ho Lee, Kwang Ryeon Park, and Yong Pyo Suh. Discussion by Donald F. Meinheit and Neil S. Anderson. Disc. 107-S27/From the May-June 2010 ACI Structural Journal, p. 282. Crack Width Estimation for Concrete Plates. Paper by H. Marzouk, M. Hossin, and A. Hussein. Discussion by Andor Windisch. Disc. 107-S32/From the May-June 2010 ACI Structural Journal, p. 330. Shear Strengths of Prestressed Concrete Beams Part 1: Experiments and Shear Design Equations. Paper by Arghadeep Laskar, Thomas T. C. Hsu, and Y. L. Mo. Discussion by Andor Windisch.