Behavior of Concrete Beams Reinforced with ASTM A1035 Grade 100 Stirrups under Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Concrete Beams Reinforced with ASTM A1035 Grade 100 Stirrups under Shear

Author(s): Aruna Munikrishna, Amr Hosny, Sami Rizkalla, and Paul Zia

Publication: Structural Journal

Volume: 108

Issue: 1

Appears on pages(s): 34-41

Keywords: beam; cracking; deflection; high-strength reinforcement; shear strength; stirrup; web reinforcement

DOI: 10.14359/51664200

Date: 1/1/2011

Abstract:
This paper presents the results of an investigation of shear strength of large-sized concrete beams reinforced with ASTM A1035 Grade 100 bars. The performance of these beams is compared to that of similar beams reinforced with ASTM A615 Grade 60 bars. The results indicate that by using the higher yield strength of ASTM A1035 bars with a reduced reinforcement ratio, the beams can achieve similar shear strengths as the beams reinforced with Grade 60 bars. The results also show that cracking and deflection under service load of the beams with a reduced reinforcement ratio are within acceptable limits.


ALSO AVAILABLE IN:

Electronic Structural Journal