Title: Effect of metakaolin on the near surface characteristics of concrete

Author(s): Rafat Siddiqe, Amandee Kaur

Publication: RILEM

Volume: 44

Issue: 1

Appears on pages(s): 77-88

Keywords: Compressive strength, Initial surface absorption, Metakaolin, Near surface characteristics, Sorptivity, Water absorption

DOI:

Date: 1/1/2011