Prototype and model masonry behaviour under different loading conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prototype and model masonry behaviour under different loading conditions

Author(s): A. Mohammed, T. Hughes

Publication: RILEM

Volume: 44

Issue: 1

Appears on pages(s): 53-65

Keywords: Strength, Model scale, Reduced scale, Mosonry, Structural behaviour, Brickwork

DOI:

Date: 1/1/2011

Abstract:
The aim of this paper is to systematically determine the effect of scale on masonry structural behaviour under various loading conditions. Small scale models have been employed to understand masonry structural behaviour over the years, because testing prototype masonry structures is both costly and challenging to undertake in a controlled laboratory environment. A programme of tests have been carried out at four scales namely prototype, half, fourth and sixth scale under five different loading conditions; compression, shear, diagonal tension, flexure and bond tension, with a view to understanding how each of these conditions affects masonry structural behaviour over the range of scales enumerated. The results show that scale or size effect is mostly pronounced in the masonry compressive strength.


International union of laboratories and experts in construction materials, systems and structures, International Partner Access

View Resource »