Title: Mechanical properties of calcium silicate hydrates

Author(s): Rouhollah Alizadeh, James Beaudoin, Laila Raki

Publication: RILEM

Volume: 44

Issue: 1

Appears on pages(s): 13-28

Keywords: Dynamic mechanical analysis, Calcuium silicate hydrate (C-S-H), Hydrated Portland cment, Nanostructure, Elasticity, Damping

DOI:

Date: 1/1/2011

Abstract:


International union of laboratories and experts in construction materials, systems and structures, International Partner Access