Title: Evaluation of surface sealers for concrete hydraulic structures exposed to low temperatures

Author(s): Jahangir Mirza, Charles Abesque, Marc-Andre Berube

Publication: RILEM

Volume: 44

Issue: 1

Appears on pages(s): 5-12

Keywords: Cold climates, Concrete hydraulic structures, Silanes, Siloxanes, Vapor transmission, Water absorption

DOI:

Date: 1/1/2011

Abstract:


International union of laboratories and experts in construction materials, systems and structures, International Partner Access