Title: The Effect of Curling on Floor Flatness

Author(s):

Publication: Concrete International

Volume: 32

Issue: 12

Appears on pages(s): 76

Keywords:

DOI:

Date: 12/1/2010

Abstract:
ACI 117-06 and ACI 117-10, “Specification for Tolerances for Concrete Construction and Materials,” require F-numbers to be measured within 72 hours after slab concrete placement.