International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of service life design models on concrete structures exposed to marine environment

Author(s): Irina Stipanovic Oslakovic, Dubravka Bjegovic, Dunja Mikulic

Publication: RILEM

Volume: 43

Issue: 10

Appears on pages(s): 1397-1412

Keywords: Chlorides, Reinforced concrete, Marine environment, Deterministic modelling, Probabilistic modelling

DOI:

Date: 10/19/2010

Abstract:


International union of laboratories and experts in construction materials, systems and structures, International Partner Access

View Resource »