Title: Investigation on the scattering-filling coarse aggregate self-consolidating concrete

Author(s): Weiguo Shen, Tao Zhang, Migkai Zhou, Zhi Cai, Jingqiang Hu, Jiasheng Li

Publication: RILEM

Volume: 43

Issue: 10

Appears on pages(s): 1343-1350

Keywords: Self-consolidating concrete, Scattering-filling coarse aggregate -process, Strength, Shrinkage, Permeability

DOI:

Date: 10/19/2010

Abstract: