Technical Committee on Autogenous Healing in Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Technical Committee on Autogenous Healing in Cementitious Materials

Author(s): Shin-ichi IGARASHI, Minoru KUNIEDA, Tomoya NISHIWAKI

Publication: JCI

Volume:

Issue:

Appears on pages(s): 91-102

Keywords: Activated repairing, automatic healing, crack, natural healing repair technique

DOI:

Date: 7/1/2009

Abstract:
The Committee on Autogenous Healing in Cementitous Materials (Chairman: Shin-ichi Igarashi, Kanazawa University) has carried out its activities to reorganize past studies on the self-healing/-repairing function of concrete over two years (2007-2008). A survey of the literature including the latest research trends of the committee members was conducted with a particular focus on the mechanism of self-healing/-repairing, in order to classify and define the phenomena. The Committee also held a workshop/panel discussion during the annual convention of JCI in 2008, at which valuable knowledge form researchers in various spheres was accumulated, with discussion made on the required direction of fortune study.