Technical Committee on Quality control testing method to assess the certainty of construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Technical Committee on Quality control testing method to assess the certainty of construction

Author(s): Toshiki AYANO, Tsuyoshi MARUYA, Masarou KOJIMA, Kimitaka UJI, Keiichi IMAMOTO, Shinji URANO, Ken-ichirou NAKARAI, Yasumichi KOSHIRO, Koichi TAKAHASHI

Publication: JCI

Volume:

Issue:

Appears on pages(s): 65-90

Keywords: Certainty of execution, concrete in the structure, filling capability, quality of cover concrete, quality test method

DOI:

Date: 7/1/2009

Abstract:
The Committee conducted research to elucidate the current state of test methods to confirm the certainty of construction execution. Availabilities of the test methods to assess that the performance of placed concrete actually meets the designed performance was investigated. Test methods to evaluate the property of concrete and their adequate timing to be applied in each execution stages were also researched/ Furthermore, a questionnaire survey was conducted a d summarized particularly regarding new test methods to evaluate the properties of concrete and test methods to confirm of various specifications agreed upon before execution are actually secured. Field tests were conducted as well to investigate the effect of execution on the in-situ qualities of concrete.