Technical Committee on Assessment of Damage and Restorability of Reinforced Concrete Structures Damaged by Earthquakes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Technical Committee on Assessment of Damage and Restorability of Reinforced Concrete Structures Damaged by Earthquakes

Author(s): Nobuaki SHIRAI, Hikaru NAKAMURA, Hideyuki KINUGASA, Susumu KONO, Kaoru KOBAYASHI

Publication: JCI

Volume:

Issue:

Appears on pages(s): 1-17

Keywords: Restorability, repair, retrofit, damage evaluation damage control, economy, mechanical capacity

DOI:

Date: 7/1/2007

Abstract:
objectives of the committee were to assess a degree of damage to be caused in reinforced concrete (hereafter refers to as RC) structures under severe earthquakes, to provide seismically safe and economical structures by means of appropriate repair and retrofit, and to establish such a seismic design method. For achieving these purposes, the committee collected and reviewed the previous works on the following items: (1) framework of the seismic design method toward better consideration of restorability, (2) current guidelines or standards relevant to the damage evaluation and control, and their applications to actually damaged structures, and (3) practical art-of-the-engineering related to the performance evaluation method of repaired and/or retrofitted structures.


Japan Concrete Institute, International Partner Access

View Resource »