Carbon-Fiber Cement-Based Materials for Electromagnetic Shielding

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Carbon-Fiber Cement-Based Materials for Electromagnetic Shielding

Author(s): Sivaraja Muthusamy and D. D. L. Chung

Publication: Materials Journal

Volume: 107

Issue: 6

Appears on pages(s): 603-611

Keywords: carbon; electrical resistivity; electromagnetic shielding; fiber; mechanical properties; silica fume; sizing

DOI: 10.14359/51664047

Date: 11/1/2010

Abstract:
Short carbon fiber is used as an admixture with silica fume to form cement-matrix composites. It is made from pitch or polyacrylonitrile (PAN). PAN-based fiber with a diameter of 7 mm is effective for providing electromagnetic interference (EMI) shielding (1 GHz), low electrical resistivity (DC), and high flexural strength and modulus. Its shielding ability is superior to that of previously studied pitch-based fiber with a diameter of 15 mm (6 × 10–4 in.). Thermally desized PAN-based fiber is less effective than the unsized counterpart for providing shielding, reflection, and low electrical resistivity, but it is more effective as a reinforcement. An increase in the fiber content increases the shielding effectiveness, decreases the resistivity; and increases the flexural strength and modulus. For each fiber content in percentage by mass of cement, the addition of sand causes a slight decrease of the shielding effectiveness; at the same fiber volume fraction, the shielding effectiveness is similar for cases with and without sand.