Four Epoxy Specifications-503.1-92, 503.2-92, 503.3-10 503.4-92

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Four Epoxy Specifications-503.1-92, 503.2-92, 503.3-10 503.4-92

Author(s): ACI Committee 503

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 20

Keywords: adhesives; aggregates; aluminum; bond (concrete to concrete); bonding; bricks; coatings; concrete construction; concrete pavements; copper; epoxy resins; fresh concretes; hardened concrete; mortars (material); quality control; repairs; resurfacing; safety

DOI:

Date: 11/1/2010

Abstract:

Note: 503.1/503.4 is only available in PDF format.

503.1-92 (Reapproved 2003): This specification describes the work of bonding hardened concrete. steel, wood, brick and other materials to hardened concrete with a multi-component epoxy adhesive such as defined for this purpose in ASTM C 881. It includes controls for adhesive labeling, storage, handling, mixing and application, surface evaluation and preparation as well as inspection and quality control. 503.2-92 (Reapproved 2003): This specification describes the work of bonding plastic concrete to hardened concrete with a multi-component epoxy adhesive such as defined speci-for this purpose in ASTM C 881. It includes controls for adhesive labeling, supple-storage, handling, mixing and application, surface evaluation and preparation as well as inspection and quality control. 503.3-10: This specification describes the work of producing a skid-resistant surface on hardened concrete by the application of a multi-component epoxy resin. It includes controls for resin labeling, storage, handling, mixing, and application; surface evaluation and preparation; and inspection and quality. In addition, it describes an aggregate to be used with the coating. 503.4-92 (Reapproved 2003): This specification describes the work of repairing defects in hardened portland cement concrete with a sand-filled mortar using an adhesive binder such as defined in ASTM C 881. It includes controls for adhesive labeling storage, handling, mixing and application, surface evaluation and preparation as well as inspection and quality control.