International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Si:Al ratio on the microstructural and mechanical properties of a fine-limestone aggregate alkali-activated slag concrete

Author(s): Aaron Sakulich, Edward Anderson, Caroline Schauer, Michael Barsoum

Publication: RILEM

Volume: 43

Issue: 7

Appears on pages(s): 1025-1035

Keywords: Slag, Alkali-activated concrete, Geopolymer, SEM

DOI:

Date: 7/1/2010

Abstract:


International union of laboratories and experts in construction materials, systems and structures, International Partner Access