Analysis of the abstraction of water from freshly mixed jointing mortars in masonry construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of the abstraction of water from freshly mixed jointing mortars in masonry construction

Author(s): C. Ince, M. Carter, M. Wilson, A. El-Turki, R. Ball, G. Allen, N. Collier

Publication: RILEM

Volume: 43

Issue: 7

Appears on pages(s): 985-992

Keywords: Mortar, Transport properties, Kinetics, Desorptivity

DOI:

Date: 7/1/2010

Abstract:
Sharp front theory is used to derive an equation describing the time taken for a wet mortar joint to be dewatered by an absorbent substrate. The equation shows that the time taken to dewater a mortar joint is directly proportional to its thickness and inversely proportional to the transfer sorptivity, itself a function of the sorptivity of the substrate and the desorptivity of the wet mix. Experimental data are presented which validate this equation and the results show that the time to dewater a mortar depends on both the hydraulicity and the initial water content of the mix. For the practically important case of jointing mortars applied in 10 mm layers to a typical facing brick we show that dewatering times range from 20 s to 1 min for Portland cement and NHL 2 mortars, respectively, and that 40–60% of the original mix water is lost in the process.


International union of laboratories and experts in construction materials, systems and structures, International Partner Access

View Resource »