Title: Freeze–thaw damage and chemical change of a portland cement concrete in the presence of diluted deicers

Author(s): Xianming Shi, Laura Fay, Marijean Peterson, M. Peterson, Zhengxian Yang

Publication: RILEM

Volume: 43

Issue: 7

Appears on pages(s): 933-946

Keywords: Deicer, Portland cement concrete, SEM, EDX, Freeze–thaw

DOI:

Date: 7/1/2010

Abstract: