Title: 364.5T-10: Importance of Modulus of Elasticity in Surface Repair Materials

Author(s): ACI Committee 364

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 3

Keywords: compatibility; cracking; creep; elastic modulus; load-carrying; repair; strain; stress; tension.

DOI:

Date: 9/1/2010

Abstract:

Note: 364.5T-10 is only available in PDF format.

Surface repairs must be dimensionally and mechanically compatible with the existing concrete substrate to minimize cracking and ensure that the repair and existing structure act monolithically. To achieve repairs that comply with these requirements, the magnitude of the repair material modulus of elasticity with respect to that of the substrate needs to be taken into account.