Title: The Cement Mill Test Report

Author(s): Dave Suchorski

Publication: Concrete International

Volume: 32

Issue: 11

Appears on pages(s): 46-49

Keywords: engineering reports, design, cement mill test report, cement specification

DOI:

Date: 11/1/2010

Abstract:
The main purpose of the cement mill test report is to certify that the produced cement meets the requirements of the applicable ASTM and AASHTO cement standards. It also gives information about the average chemical and physical properties of the cement produced during a particular production period—a period that can span from a few days up to a full month. This article details what a design engineer should look for in a cement mill test report.