Precision of Compressive Strength Testing of Concrete with Different Cylinder Specimen Sizes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precision of Compressive Strength Testing of Concrete with Different Cylinder Specimen Sizes

Author(s): Hosein Taghaddos, Hamid R. Soleymani, and J. D. (Dave) Robson

Publication: Materials Journal

Volume: 107

Issue: 5

Appears on pages(s): 461-468

Keywords: compressive strength; cylinders; index; size; specimen; repeatability; reproducibility

DOI: 10.14359/51663965

Date: 9/1/2010

Abstract:
Most standardization agencies allow small-cylinder specimens (100 x 200 mm [4 x 8 in.]) to be used in compressive strength concrete testing. Some engineers are still skeptical about using small cylinders, however, as they believe that compressive strength testing results from small cylinders are too varied. Limited studies have been conducted regarding the precision of small cylinders compared to precision studies for conventional cylinders (150 x 300 mm [6 x 12 in.]). This paper describes the results of a comparative concrete testing program conducted by 15 laboratories in Edmonton, AB, Canada, over the past 10 years. This study attempted to develop within-laboratory (repeatability) and between-laboratory (reproducibility) precision indexes for small and conventional concrete specimens by analyzing more than 2700 compressive strength concrete testing data within a compressive strength range of 17 to 57 MPa (2500 to 8300 psi).


ALSO AVAILABLE IN:

Electronic Materials Journal