Precast Technology Creates High-Quality, Two-Sided Molded Panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precast Technology Creates High-Quality, Two-Sided Molded Panels

Author(s): Tom Kuckhahn

Publication: Concrete International

Volume: 32

Issue: 10

Appears on pages(s): 51-53

Keywords: precast concrete, precast panels, molded panels, formwork

DOI:

Date: 10/1/2010

Abstract:
After considerable investment in research and development, Verti-Crete developed an innovative mold-and-form system for precasting multiple walls in a vertical gang form. The result is a molded stone pattern on both sides of the wall and a production system that turns out more walls in less time and at a lower cost than traditional methods. Ideally suited to surround individual homes or businesses or to create an attractive entrance for parks, communities, and neighborhood associations, the panels can be scaled to meet a variety of project sizes and are engineered to meet the building codes of almost any area.