ITG-6R-10: Design Guide for the Use of ASTM A1035/A1035M Grade 100 (690) Steel Bars for Structural Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ITG-6R-10: Design Guide for the Use of ASTM A1035/A1035M Grade 100 (690) Steel Bars for Structural Concrete

Author(s): ACI Committee 93

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 90

Keywords: bar; concrete; design; guide; high-strength steel; structural.

DOI:

Date: 8/1/2010

Abstract:
This guide provides recommendations on design provisions for the use of ASTM A1035/ASTM1035M Grade 100 (690) deformed steel bars for reinforced concrete members. The recommendations address only those requirements of ACI 318-08 that limit efficient use of such steel bars. Other code requirements are not affected. This guide includes a discussion of the material characteristics of Grade100 (690) ASTM A1035/A1035M deformed steel bars and recommends design criteria for beams, columns, slab systems, walls, and footings for Seismic Design Category (SDC) A, B, or C, and also for structural components not designated as part of the seismic-force-resisting system for SDC D, E, or F.