Corrosion Protection of Fiber-Reinforced Polymer-Wrapped Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Corrosion Protection of Fiber-Reinforced Polymer-Wrapped Reinforced Concrete

Author(s): Sangeeta Gadve, Abhijit Mukherjee, and S. N. Malhotra

Publication: Materials Journal

Volume: 107

Issue: 4

Appears on pages(s): 349-356

Keywords: active protection; anodic current; corrosion; fiber-reinforced polymer; flexure strength; mass loss; passive protection; reinforced concrete

DOI: 10.14359/51663860

Date: 7/1/2010

Abstract:
Reinforced concrete (RC) flexure members such as bridges, slabs, and beams that have been damaged due to the corrosion of steel reinforcement are often rehabilitated with fiber-reinforced polymer (FRP) composites. This paper investigates passive as well as active protection of the steel reinforcing bar in RC flexure members that are treated with surface bonded FRP. Passive protection is investigated using glass FRP (GFRP) and carbon FRP (CFRP) sheets that have been adhesively bonded to the beam specimens. Active protection has been studied using electrically conductive carbon fiber wraparounds as an anode while the reinforcing bar is used as a cathode. Accelerated corrosion is inflicted in RC beams by immersing them in saltwater and passing anodic current through the reinforcement. For investigating active protection, the adhesive has been modified to impart electrical conductivity. Specimens were exposed to a highly corrosive environment for a specified time. Flexure strength, mass loss, and half-cell potential are reported as metrics of performance of the samples. The proposed technique has been very effective in retarding the corrosion of steel.