SP-271: Structural Concrete in Performance-Based Seismic Design of Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-271: Structural Concrete in Performance-Based Seismic Design of Bridges

Author(s): Editors: Pedro F. Silva & Raj Valluvan / Sponsored by: ACI Committee 341

Publication: Symposium Paper

Volume: 271

Issue:

Appears on pages(s): 155

Keywords:

DOI: 10.14359/51663851

Date: 7/1/2010

Abstract:
This CD-ROM consists of seven papers that were presented at a session sponsored by ACI Committee 341 at the ACI Fall Convention in St. Louis, MO, in November 2008. The papers focus on the most recent advancements in performance-based seismic design of reinforced concrete bridges, including analytical and experimental studies, and design and construction practices with relevant information related to reinforced concrete bridges based on performance-based design. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-271




  