546.2R-10: Guide to Underwater Repair of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 546.2R-10: Guide to Underwater Repair of Concrete

Author(s): ACI Committee 546

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 32

Keywords: anti-washout; cathodic protection; concrete removal; deterioration; diver; formwork; marine placement; pile-jackets; polymer(s); repair; surface preparation; tremie; underwater.

DOI:

Date: 6/1/2010

Abstract:
This document provides guidance on the selection and application of materials and methods for the repair and strengthening of concrete structures under water. An overview of materials and methods for underwater repair is presented as a guide for making a selection for a particular application. References are provided for additional information about selected materials and construction methods.