423.9M-10 Test Method for Bleed Stability of Cementitious Post-Tensioning Tendon Grout

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 423.9M-10 Test Method for Bleed Stability of Cementitious Post-Tensioning Tendon Grout

Author(s): Joint ACI-ASCE Committee 423

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 3

Keywords: bleeding; bleed stability; bleed water; grout; post-tensioning; pressure.

DOI:

Date: 6/1/2010

Abstract:

Note: 423.9M-10 is only available in PDF format.

Cement grouts for post-tensioning tendons ensure durability of the system. Voids formed from bleeding of grout may result in loss of a protective environment that may lead to corrosion of prestressing steel. This test method is a tool to evaluate the bleed stability of a grout under static pressure and can be used to prequalify grout materials or for quality control.