International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of engineered cementitious composites with limestone powder and blast furnace slag

Author(s):

Publication: RILEM

Volume: 43

Issue: 6

Appears on pages(s):

Keywords: Engineered cementitious composites; Polyvinyl alcohol; Blast furnace slag; Calcium carbonate;Environmental scanning electron microscopy; Backscattered electron; Portland cement-to-BFS

DOI:

Date: 5/26/2010

Abstract:


International union of laboratories and experts in construction materials, systems and structures, International Partner Access