Prediction of solid block masonry prism compressive strength using FE model

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prediction of solid block masonry prism compressive strength using FE model

Author(s): CH. Uday Vyas, V. Uday Vyas, B. Venkatarama Reddy, V. Venkatarama Reddy

Publication: RILEM

Volume: 43

Issue: 5

Appears on pages(s): 719-735

Keywords:

DOI:

Date: 5/10/2010

Abstract:
Masonry strength is dependent upon characteristics of the masonry unit, the mortar and the bond between them. Empirical formulae as well as analytical and finite element (FE) models have been developed to predict structural behaviour of masonry. This paper is focused on developing a three dimensional non-linear FE model based on micro-modelling approach to predict masonry prism compressive strength and crack pattern. The proposed FE model uses multi-linear stress–strain relationships to model the non-linear behaviour of solid masonry unit and the mortar. Willam–Warnke’s five parameter failure theory developed for modelling the tri-axial behaviour of concrete has been adopted to model the failure of masonry materials. The post failure regime has been modelled by applying orthotropic constitutive equations based on the smeared crack approach. Compressive strength of the masonry prism predicted by the proposed FE model has been compared with experimental values as well as the values predicted by other failure theories and Eurocode formula. The crack pattern predicted by the FE model shows vertical splitting cracks in the prism. The FE model predicts the ultimate failure compressive stress close to 85% of the mean experimental compressive strength value.