FRC—Rheology, Fiber Dispersion, and Mechanical Properties

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: FRC—Rheology, Fiber Dispersion, and Mechanical Properties

Author(s): N. Ozyurt, T. O. Mason, and S. P. Shah

Publication: Symposium Paper

Volume: 268

Issue:

Appears on pages(s): 173-182

Keywords: AC-impedance spectroscopy; fiber dispersion; rheology; viscosity-modifying agent.

DOI: 10.14359/51663717

Date: 3/1/2010

Abstract:
The effects of fresh state properties on the fiber dispersion characteristics of fiber-reinforced composites (FRCs) were studied by quantifying fiber segregation. Fresh state properties of concrete mixes were varied using different combinations of a plasticizing agent and viscosity modifier. A self-designed parallel-plate rheometer was used to obtain rheological parameters. Vibration was applied to the specimens and vibration times were varied to understand the effects of vibration on fiber segregation. An electrical characterization method, alternating current-impedance spectroscopy (AC-IS), was used to quantify fiber segregation in specimens. The relationship between fresh state properties and fiber segregation was evaluated.