440.7R-10: Guide for the Design and Construction of Externally Bonded Fiber-Reinforced Polymer Systems for Strengthening Unreinforced Masonry Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 440.7R-10: Guide for the Design and Construction of Externally Bonded Fiber-Reinforced Polymer Systems for Strengthening Unreinforced Masonry Structures

Author(s): ACI Committee 440

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 46

Keywords: buildings; cracking; cyclic loading; detailing; earthquake resistance; fiber-reinforced polymers; fibers; flexure; masonry; shear; structural analysis; structural design; unreinforced.

DOI:

Date: 4/1/2010

Abstract:
Fiber-reinforced polymer (FRP) systems are an option to consider for strengthening unreinforced masonry (URM) structures. Traditional strengthening systems include external steel plates, reinforced concrete (RC) overlays, span shortening with steel subframing or bracing, and internal steel reinforcement. Relative to traditional systems, features of FRP systems include high tensile strength, light weight, ease of construction, and resistance to corrosion. This guide offers general information on FRP systems use, a description of their unique material properties, and recommendations for the design, construction, and inspection of FRP systems for strengthening URM structures. These guidelines are based on knowledge gained from a comprehensive review of experimental and analytical investigations and field applications.