Early age volume change of cement asphalt mortar in the presence of aluminum powder

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Early age volume change of cement asphalt mortar in the presence of aluminum powder

Author(s): Fazhou Wang, Zhichao Liu, Shuguang Hu

Publication: RILEM

Volume: 43

Issue: 4

Appears on pages(s): 493-498

Keywords: Cement asphalt mortar, Volume change, Aluminum powder, Temperature

DOI:

Date: 4/6/2010

Abstract:
Cement asphalt mortar (CA mortar) is a highly flowable grouting material used in the slab track structure. CA mortar is required to possess a volume expansion rate of 1.0–3.0% after 24 h to guarantee a desired filling effect. This is achieved by the incorporation of aluminum powder (AP). The article investigates the volume change of CA mortar under various AP dosages, temperatures and asphalt emulsion/cement ratio (A/C). Results indicate that when AP is absent, volume shrinkage of 1.8–3.0% is noted at temperatures of 10–30°C; upon the addition of 0.013–0.021% AP, CA mortar undergoes slight volume shrinkage before 4 h, and then keeps expanding until about 24 h after which volume expansion slows down gradually; the expansion rate of CA mortar is greater, the lower the temperature is, and also the higher A/C is.


International union of laboratories and experts in construction materials, systems and structures, International Partner Access

View Resource »