Design methods for fibre-reinforced concrete: A state-of-the-art review

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design methods for fibre-reinforced concrete: A state-of-the-art review

Author(s): Anette Jansson, Kent Gylltoft & Ingemar Löfgren

Publication: NCR

Volume: 38

Issue: 2

Appears on pages(s): 31-46

Keywords: Fibre-reinforced concrete, lightweight concrete, four-point bending test, finite element analysis

DOI:

Date: 12/17/2008

Abstract:
The increasing interest in the use of fibre reinforcement has created a need for established design and analysis methods. Fibre reinforcement is mainly used in applications such as industrial floors and sprayed concrete, although other application areas exist. Apart from increased load-carrying capacity, one of the main benefits of adding fibres to concrete is the potential reduction in crack width, which depends on the amount of fibres added and positively affects the durability of the finished structure. By comparing ten design methods proposed by technical committees, this paper provides a basis for further research aimed at developing a common design basis. Evaluation is based on the way the fibre capacity is considered. In addition, a "good" design method should also consider all (or most) design situations. It was found that, for design, the Italian proposal provides comprehensiveness. However, some amendments are needed, e.g. a suggestion is that the proposed formula for calculating crack width/crack spacing should be modified to include the residual tensile strength.