FEM simulations of reinforced concrete beams attacked by corrosion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: FEM simulations of reinforced concrete beams attacked by corrosion

Author(s): Irina Sæther, Bjørnar Sand

Publication: NCR

Volume: 39

Issue: 2

Appears on pages(s): 15-31

Keywords: Cocncrete, finite element analysis, corroding steel bars, DIANA

DOI:

Date: 6/15/2012

Abstract:
The present work is devoted to the application of finite element analysis to simulate the mechanical behaviour of reinforced concrete members with corroding steel bars using the finite element program DIANA. In the present approach only the effects of corrosion are taken into consideration. Accordingly, loss of steel bar section, and reduced bond between deteriorated concrete and corroded rebar are accounted for in the present work. The results of the simulations are validated against published results from laboratory tests on medium scale beams. The load-deflection behaviour obtained from the finite element simulations are in agreement with the test data.