Predicting Model for Pore Structure of Concrete Including Interface Transition Zone between Aggregate and Cement Paste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Predicting Model for Pore Structure of Concrete Including Interface Transition Zone between Aggregate and Cement Paste

Author(s): Gi-Sung Pang, Sung Tae Chae, and Sung Pil Chang

Publication: IJCSM

Volume: 3

Issue: 2

Appears on pages(s): 81-90

Keywords: porosity; microstructure; interface transition zone; durability; service life

DOI:

Date: 12/31/2009

Abstract:
This paper proposes a semi analytical model to describe the pore structure of concrete by a set of simple equations. The relationship between the porosity and the microstructure of concrete has been considered when constructing the analytical model. The microstructure includes the interface transition zone (ITZ) between aggregates and cement paste. The predicting model of porosity was developed with considering the ITZ for various mixing of mortar and concrete. The proposed model is validated by the rapid experimental programs. Although the proposed model is semi-analytical and relatively simple, this model could be reasonably utilized for the durability design and adapted for predicting the service life of concrete structures.