Modeling of Reinforced Concrete Slabs Strengthened with Fiber-Reinforced Polymer or Steel Plates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling of Reinforced Concrete Slabs Strengthened with Fiber-Reinforced Polymer or Steel Plates

Author(s): Usama Ebead and Huda Saeed

Publication: Structural Journal

Volume: 107

Issue: 2

Appears on pages(s): 218-227

Keywords: fiber-reinforced polymer; finite element analysis; interfacial behavior; steel bolts; steel plates; strengthening; two-way slabs.

DOI: 10.14359/51663538

Date: 3/1/2010

Abstract:
This research aims to create precise finite element models for strengthened two-way slab-column connections. The connections are categorized according to the strengthening type as flexural or punching shear specimens. Two different strengthening techniques are modeled using steel plates or fiber-reinforced polymer (FRP) strips or laminates. FRP-strengthened connections are subjected to central axial loads. The connections that use an assembly of steel plates and bolts are subjected to a central load or a combination of central load and moment. The three-dimensional (3D) assembly of the slab and column of the connections is simulated. In addition, the interfacial behavior between the FRP materials and concrete is taken into account. Furthermore, a user-defined subroutine for the microplane model for concrete is incorporated in the finite element package. Results are presented in terms of the ultimate load capacities, load-slip relationships, load-interfacial stress relationships, and stress distributions in the strengthening materials.