Compression Lap Splice in Unconfined Concrete of 40 and 60 MPa (5800 and 8700 psi) Compressive Strengths

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compression Lap Splice in Unconfined Concrete of 40 and 60 MPa (5800 and 8700 psi) Compressive Strengths

Author(s): Sung-Chul Chun, Sung-Ho Lee, and Bohwan Oh

Publication: Structural Journal

Volume: 107

Issue: 2

Appears on pages(s): 170-178

Keywords: bond; compression lap splice; end bearing; splice strength; unconfined concrete.

DOI: 10.14359/51663533

Date: 3/1/2010

Abstract:
A compression lap splice may be calculated to be longer than a tension lap splice in high-strength concrete according to current design codes. New criteria for the compression lap splice, including the effects of concrete strength and end bearing, are required. An experimental study was conducted using compressive concrete strengths of 40 and 60 MPa (5800 and 8700 psi) without transverse reinforcement. Test results showed that the splice strength was proportional to vfc' and that the spacing between bars had little effect on the splice strength. The bar stresses developed by bond were nearly identical to those calculated by the ACI Committee 408 equation. Therefore, the strength increase in the compression splices is solely attributed to end bearing. A design equation was derived for compression lap splices without transverse reinforcement through regression analysis.