Concrete Sustainability Forum

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Sustainability Forum

Author(s): Koji Sakai, Julie K. Buffenbarger, and Richard D. Stehly

Publication: Concrete International

Volume: 32

Issue: 3

Appears on pages(s): 55-59

Keywords: concrete sector, sustainability, standardization

DOI:

Date: 3/1/2010

Abstract:
ACI hosted a special event, the Concrete Sustainability Forum, immediately before its Fall 2009 convention. Topics included new initiatives within the U.S. concrete sector, sustainability activities in concrete-related organizations throughout the world, advanced sustainability technologies, and ISO standardization of sustainability for the concrete industry. During discussions that followed the presentations, participants agreed that sustainability must be a priority for the concrete industry. Declarations based on the forum and discussion called for collection and distribution of information on sustainable concrete technologies around the world, the accelerated development of sustainable concrete technologies, and continuation of the Concrete Sustainability Forum.