FRP Super Laminates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: FRP Super Laminates

Author(s): Mo Ehsani

Publication: Concrete International

Volume: 32

Issue: 3

Appears on pages(s): 49-53

Keywords: FRP, laminate, epoxy putty, strengthening

DOI:

Date: 3/1/2010

Abstract:
FRP products come in two categories: fabrics and pre-cured laminates. Fabrics offer the widest versatility in the field and are installed using the wet layup method. Pre-cured laminates are available as composite rods or narrow unidirectional strips from 3 to 10 in. (75 to 250 mm) wide and 0.05 in. (1.3 mm) thick. Laminate strips are bonded to the exterior surface of the structural element using epoxy putty. Super laminates are a new, third category of FRP product available as a 60 in. (1524 mm) wide, pre-cured composites with unidirectional or biaxial fabric reinforcement. Applications for super laminates include strengthening of pipes, production of seamless shells around existing columns or underwater piles, and strengthening of tanks and silos.




  

Edit Module Settings to define Page Content Reviewer