Title: Concrete: Yesterday, Today & Tomorrow - A Century of Concrete Ties

Author(s): Amir N. Hanna

Publication: Concrete International

Volume: 12

Issue: 8

Appears on pages(s): 52-53

Keywords:

DOI:

Date: 8/1/1990

Abstract:
It has been more than a century since concrete was first considered as a material for railroad ties. Designs were introduced in 1884 and the first concrete ties were installed in the u.s. in 1893 by the Reading Company in Germantown, Pennsylvania.