Damage of concrete in a very high stress state: experimental investigation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Damage of concrete in a very high stress state: experimental investigation

Author(s): C. Poinard, Y. Malecot, L. Malecot

Publication: RILEM

Volume: 43

Issue: 1

Appears on pages(s): 15-29

Keywords: Concrete, Triaxial test, High confining pressure, Unloading–reloading cycles, Young’s modulus, Poisson’s ratio

DOI:

Date: 12/1/2009

Abstract:
This study is intended to characterize the evolution in triaxial behavior of a standard concrete subjected to confining pressures varying from 0 to 600 MPa. Hydrostatic and triaxial tests, with several unloading–reloading cycles, are carried out on concrete samples using a high-capacity triaxial press. These tests serve to identify the evolution of the elastic unloading characteristics of concrete, depending on both confining pressure and axial strain. A number of optical observations are also provided to allow visualizing the evolution in concrete damage mode in the middle of the sample. Experimental results indicate a sizable change in concrete behavior with confining pressure. At low pressure values, Young’s modulus decreases and Poisson’s ratio rises sharply with axial strain. The concrete exhibits brittle behavior with failure caused by a localized damage mechanism. In contrast, at high confining pressures, the concrete becomes a ductile material, and the evolution in its unloading characteristics is negligible. Failure is thus associated with diffuse material damage. The concrete behaves like a granular material controlled by plasticity, meaning that the damage phenomenon observed at low confinement is completely inhibited.