Pushover Analysis of Shear-Critical Frames: Formulation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pushover Analysis of Shear-Critical Frames: Formulation

Author(s): Serhan Guner and Frank J. Vecchio

Publication: Structural Journal

Volume: 107

Issue: 1

Appears on pages(s): 63-71

Keywords: beam column; fiber model; frame structure; monotonic; nonlinear analysis; pushover; reinforced concrete; retrofit; shear.

DOI: 10.14359/51663389

Date: 1/1/2010

Abstract:
An analytical procedure is presented for the nonlinear analysis of reinforced concrete frame structures consisting of beams, columns, and shear walls under monotonic and pushover loads. The procedure is capable of accurately representing shear-related mechanisms coupled with flexural and axial behaviors. The formulation described herein uses linear-elastic frame analysis algorithms in a nonlinear mode based on an unbalanced force approach. Rigorous nonlinear sectional analyses of concrete member cross sections, using a distributed-nonlinearity fiber model, are performed based on the disturbed stress field model. The proposed method is distinct from existing methods in that it allows for the inherent and accurate consideration of shear effects and significant second-order mechanisms within a simple modeling process suitable for practical applications. Decisions regarding the anticipated behavior and failure mode or the selection of appropriate analysis options and parameter values, or additional supporting calculations such as the moment-axial force or shear force-shear deformation responses, are not required.