549.3R-09: Report on Glass Fiber-Reinforced Concrete Premix (Reapproved 2017)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 549.3R-09: Report on Glass Fiber-Reinforced Concrete Premix (Reapproved 2017)

Author(s): ACI Committee 549

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 24

Keywords: cement-based composites; cement boards; cement panels; composite materials; concrete panels; ductility; durability; engineering properties; fiber-reinforced cement-based materials; ferrocement; fibers; flexural strength; glass fiber-reinforced concrete.

DOI:

Date: 12/1/2009

Abstract:
Glass fiber-reinforced concrete premix technology is becoming increasingly popular worldwide for manufacture of precast concrete products used in industrial, architectural, civil engineering, and construction applications. Glass fiber-reinforced concrete premix products provide a useful balance of properties such as strength, toughness, durability, moisture resistance, dimensional stability, fire resistance, and aesthetics. This report summarizes the current knowledge of materials, manufacturing methods, engineering properties, and applications of glass fiber-reinforced concrete premix.