Development and analysis of high performance hybrid cement composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development and analysis of high performance hybrid cement composites

Author(s): V. J. FERRARI, J. B. DE HANAI

Publication: IBRACON

Volume: 2

Issue: 3

Appears on pages(s): 254-261

Keywords: cementitious composites, hybridization, flexional tougheness, fracture toughness.

DOI:

Date: 10/1/2009

Abstract:
In this work, the hybridization effect in cimentitious composites is studied in an attempt to modify the material and to improve the process of transference of stress of the matrix to steel fibers. Steel short fibers and steel microfibers were used in a mortar matrix for production of notched beams of 150 mm x 150 mm cross section with a length of 500 mm. Tests in beams under three point loading were conducted with crack mouth opening displacement (CMOD) control. The performance of the hybrid composites were compared with the performances of steel short fibre composites and matrix. The results were analised considering the flexional toughness and fracture tougheness parameters. The hybridization process have shown to have a satisfactory behavior translated for a strain hardening.