Analytical solution to simulate the behavior of reinforced concrete beams post-strengthened with FRP strips

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analytical solution to simulate the behavior of reinforced concrete beams post-strengthened with FRP strips

Author(s): M. R. GARCEZ, L. C. P. DA SILVA FILHO

Publication: IBRACON

Volume: 2

Issue: 3

Appears on pages(s): 222-232

Keywords: FRP, tri-linear analysis, analytical solution.

DOI:

Date: 10/1/2009

Abstract:
Aiming to develop an analytical solution to describe the behavior of reinforced concrete beams post-strengthened with FRP systems, with or without prestressing, a non-linear solution based on a tri-linear moment-curvature response was proposed. Three characteristic points