Interactions Between Comb-Type Superplasticizers and Slag Cement Pastes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Interactions Between Comb-Type Superplasticizers and Slag Cement Pastes

Author(s): L. Regnaud, R. Alfani, A. Vichot, B. Le Rolland, and E. Borgarello

Publication: Symposium Paper

Volume: 262

Issue:

Appears on pages(s): 139-152

Keywords: adsorption; blast-furnace slag; comb-type superplasticizer; dispersion; hydration; interaction; polycarboxylate polymer (PCP); slag cement; sulfate.

DOI: 10.14359/51663228

Date: 10/1/2009

Abstract:
Comb-type superplasticizers are widely used for producing self-compacting or high-strength concrete. Recently, slag cement binders have been developed for their contribution to sustainable development and for their capacity to improve the durability of concrete. In order to enhance the use of slag cements in concrete formulation, it appears important to progress in the knowledge of their interaction with comb-type superplasticizers. In this way, this paper discusses about the polymer adsorption capacity on blast furnace slag and laboratory prepared mixes of slag and cement compared with portland cement. We observed that the substitution of cement with a very slow reactive binder like slag at early age, which induces then a different polymer adsorption capacity, allows to obtain a polymer adsorption less sensitive towards sulphate ions concentration. Besides, we observed that the dispersing effect of polycarboxylate polymer (PCP) was higher on slag cement paste than on portland cement paste. Therefore, slag cements seem to be interesting in concrete formulation because their interactions with superplasticizer seem to be less affected by the chemical composition of cement, and the superplasticizer effect is enhanced.