Title: Shear Friction of Reinforced Self-Compacting Concrete Members

Author(s): P. Desnerck, G. De Schutter, and L. Taerwe

Publication: Symposium Paper

Volume: 261

Issue:

Appears on pages(s): 133-141

Keywords: aggregate interlock; push-off; self-compacting concrete (SCC); shear friction.

DOI: 10.14359/51663206

Date: 10/1/2009

Abstract:
Aggregate interlock along inclined cracks is one of the basic mechanisms which contributes to the shear resistance of reinforced concrete members. In self-compacting-concrete (SCC) the amount of coarse aggregates is lower than in conventional vibrated concrete (CVC). This different grading could have an influence on the aggregate interlock. To study this effect, push-off tests are carried out. The shear plane of the specimen is crossed by steel bars resulting in reinforcement ratios ranging between 0.45 and 2.68%. It follows that the experimentally determined shear friction of self-compacting concrete is slightly higher than the shear friction of CVC. However, the vertical displacement corresponding with the ultimate shear strength is larger.