Cracking in Reinforced Concrete Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cracking in Reinforced Concrete Buildings

Author(s): M.G. Richardson

Publication: Concrete International

Volume: 9

Issue: 1

Appears on pages(s): 21-23

Keywords:

DOI:

Date: 1/1/1987

Abstract:
Causes of cracking are detailed.