Abstract:
The material published in the previous Detailing Corner (V. 31, No. 9, Sept. 2009, pp. 43-45), led to requests for information. This month’s Detailing Corner provides responses, including detailing recommendations for walls in which larger horizontal moments will develop at wall joints, an explanation of the "0 in." dimension, and a discussion of lap splicing hooks.