No More Pour Strips

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: No More Pour Strips

Author(s): Sam Eskildsen, Mike Jones, and Jim Richardson

Publication: Concrete International

Volume: 31

Issue: 10

Appears on pages(s): 42-47

Keywords: shrinkage compensating concrete, pour strip, shrinkage, schedule.

DOI:

Date: 10/1/2009

Abstract:
A five-story, 345,000 ft2 (32,050 m2) student housing facility was built atop a three level, 600 x 270 ft (183 x 83 m), 1017-space parking structure. Although the post-tensioned parking structure had only one expansion joint, the design and construction team was able to construct the structure using no pour strips. Instead, shrinkage compensating concrete (SCC) was used to minimize slab cracking and reduce the construction schedule. Unique aspects of the analysis, design, and construction of the structures are described, with particular emphasis on the effects of SCC. Strain measurements from the structure and test blocks show that after an initial expansion, the SCC exhibited less shrinkage than would be predicted for a normal concrete mixture.