CRSI Detailing Corner: Corner Details for Wall Horizontal Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: CRSI Detailing Corner: Corner Details for Wall Horizontal Bars

Author(s): CRSI Staff

Publication: Concrete International

Volume: 31

Issue: 9

Appears on pages(s): 43-45

Keywords: intersections, continuity, hook, bar curtains

DOI:

Date: 9/1/2009

Abstract:
Ensuring continuity of horizontal reinforcing bars at wall intersections requires the consideration of splice details. Horizontal reinforcing bars at wall intersections can be hooked at one or both ends, but long bars with hooks are difficult to handle. They may also make it difficult to meet cover requirements, and they can hurt project efficiencies by making it difficult to produce, handle, and install prefabricated bar curtains. In contrast, short bars with hooks may be practical alternatives for smaller structures. Illustrations of constructible details are provided.